Caustic embrittlement is a form of stress corrosion cracking characterized by surface-initiated cracks that occur in piping and equipment exposed to caustic, primarily adjacent to non-PWHT welds. Which of the following materials is the most resistant to embrittlement?

Caustic embrittlement is a form of stress corrosion cracking characterized by surface-initiated cracks that occur in piping and equipment exposed to caustic, primarily adjacent to non-PWHT welds. Which of the following materials is the most resistant to embrittlement?
A . Carbon steel
B . Nickel based alloys
C . Low alloy steels
D . 400 Series SS

Answer: B